Investigation on Thermal Aging of HVDC XLPE
- DOI
- 10.2991/icadme-15.2015.86How to use a DOI?
- Keywords
- Cross-linked polyethylene, thermal aging, assessment techniques, activation energy.
- Abstract
HVDC XLPE cables were widely used in the transmission line for the excellent characteristics. The thermal aging properties of HVDC XLPE insulation were investigated in this work, based on different assessment techniques, such as IR Prestige-21 Infrared Spectrometer, Thermo-Gravimetric Analyzer, and X-Ray Diffractometer. It was found that, the molecular structure of XLPE cable insulation changed during the thermal aging process, carbonyl deposed as the increase of aging time and the increase of aging temperature. There was one fastest decomposition temperature for un-aged specimen and specimen aged at low temperature, while there were multiple decomposition temperatures for specimens aged at high temperature. Numerous new chemical bonds, whose activation energies differ from that of XLPE, arise during the high temperature aging. The XLPE crystallinity increased during low-temperature aging while decreased during high-temperature aging. Low-temperature is conducive to the transition of amorphous region into crystallization region, while high-temperature has damaging effect on the crystallization region.
- Copyright
- © 2015, the Authors. Published by Atlantis Press.
- Open Access
- This is an open access article distributed under the CC BY-NC license (http://creativecommons.org/licenses/by-nc/4.0/).
Cite this article
TY - CONF AU - Weiwei Li AU - Qiang Shi AU - Wei Xiao PY - 2015/10 DA - 2015/10 TI - Investigation on Thermal Aging of HVDC XLPE BT - Proceedings of the 5th International Conference on Advanced Design and Manufacturing Engineering PB - Atlantis Press SP - 428 EP - 432 SN - 2352-5401 UR - https://doi.org/10.2991/icadme-15.2015.86 DO - 10.2991/icadme-15.2015.86 ID - Li2015/10 ER -