Preparation and Application of Composite Lightweight Aggregate Concrete Self-Insulation Block
- DOI
- 10.2991/icache-15.2015.21How to use a DOI?
- Keywords
- Composite Lightweight Aggregate Concrete, Self-insulation Block, Preparation, Application
- Abstract
The composite lightweight aggregate concrete self-insulation block is prepared by pumice, polystyrene particles and other materials. The self-insulation block has dumbbell-shaped hole filled with polystyrene foam. Its preparation and molding process are studied in the test. The self-insulation blocks are applied to infilled walls in frame structure. The results show that the self-insulation block of composite lightweight aggregate concrete is with the hollow rate of 54.1%, heat resistance of 2.177 (m²•K)/W, a density of 642.29kg/m3, compressive strength of 3.96MPa. The self-insulation blocks meet exterior wall energy requirements and mechanical requirements in severe cold zones and the blocks are suitable for application.
- Copyright
- © 2015, the Authors. Published by Atlantis Press.
- Open Access
- This is an open access article distributed under the CC BY-NC license (http://creativecommons.org/licenses/by-nc/4.0/).
Cite this article
TY - CONF AU - Jiansuo Ma AU - Miaomiao Zhou AU - Huanqin Cai AU - Runshan Bai PY - 2015/11 DA - 2015/11 TI - Preparation and Application of Composite Lightweight Aggregate Concrete Self-Insulation Block BT - Proceedings of the 2015 International Conference on Architectural, Civil and Hydraulics Engineering PB - Atlantis Press SP - 102 EP - 105 SN - 2352-5401 UR - https://doi.org/10.2991/icache-15.2015.21 DO - 10.2991/icache-15.2015.21 ID - Ma2015/11 ER -