The Effect of Shell as a Substitution of Coard Aggregate with Superplasticizer Additional on the Compression Strength of Concrete

Authors
Lina Flaviana Tilik1, *, Bambang Hidayat Fuady1, Suhadi Suhadi1, Rosy Armaini1, Fadhila Firdausa1, Muhammad Rifqi Agusri1, Puji Hartoyo1
1Sriwijaya State Polytechnic
*Corresponding author. Email: lina_tilik@yahoo.co.id
Corresponding Author
Lina Flaviana Tilik
Available Online 14 February 2022.
DOI
10.2991/ahe.k.220205.003How to use a DOI?
Keywords
compressive strength; Blood clam shell; Superplasticizer
Abstract

Concrete is a type of building structure material, both buildings, bridges, and roads. Concrete is a construction material obtained from mixing sand, gravel, or crushed stone, cement, and water. To improve the properties of concrete, several kinds of additives that have certain functions are added to the concrete mixture, to improve or improve the properties of concrete, namely increasing the workability, durability, and hardening time of the concrete. Shells with excellent quality and shape are used as craft materials, while bad shapes can cause waste which results in a series of other problems, especially the cleanliness of the surrounding environment. This study aims to determine the effect of shells as a substitution of coarse aggregate with superplasticizer added material on the compressive strength of concrete. The specimens used were cylindrical with a diameter of 15 cm and a height of 30 cm. The composition of the shells determined in this study was 0%, 5%, 10%, 15%, 20% and 0.5% superplasticizer added. The planned concrete quality is Fc = 25MPa. The value of the compressive strength of concrete increased with the addition of shells by 5% and decreased in the addition of shells above 5% with 0.5% superplasticizer added. The compressive strength of normal concrete and 0.5% superplasticizer concrete is 28.26 MPa and 29.15 MPa at the age of 28 days and the compressive strength of shell concrete with a composition of 5%, 10%, 15%, and 20% added with superplasticizer 0,5% produces a compressive strength of 30.78MPa; 26.78MPa; 24.71 MPa, and 22.93 MPa at the age of 28 days.

Copyright
© 2022 The Authors. Published by Atlantis Press International B.V.
Open Access
This is an open access article under the CC BY-NC license.

Download article (PDF)

Volume Title
Proceedings of the 5th FIRST T1 T2 2021 International Conference (FIRST-T1-T2 2021)
Series
Atlantis Highlights in Engineering
Publication Date
14 February 2022
ISBN
978-94-6239-535-0
ISSN
2589-4943
DOI
10.2991/ahe.k.220205.003How to use a DOI?
Copyright
© 2022 The Authors. Published by Atlantis Press International B.V.
Open Access
This is an open access article under the CC BY-NC license.

Cite this article

TY  - CONF
AU  - Lina Flaviana Tilik
AU  - Bambang Hidayat Fuady
AU  - Suhadi  Suhadi
AU  - Rosy Armaini
AU  - Fadhila Firdausa
AU  - Muhammad Rifqi Agusri
AU  - Puji Hartoyo
PY  - 2022
DA  - 2022/02/14
TI  - The Effect of Shell as a Substitution of Coard Aggregate with Superplasticizer Additional on the Compression Strength of Concrete
BT  - Proceedings of the 5th FIRST T1 T2 2021 International Conference (FIRST-T1-T2 2021)
PB  - Atlantis Press
SP  - 13
EP  - 18
SN  - 2589-4943
UR  - https://doi.org/10.2991/ahe.k.220205.003
DO  - 10.2991/ahe.k.220205.003
ID  - Tilik2022
ER  -