Photocatalytic Heteropolyacid/CdS (HPA/CdS) Composite for Degradation of Safranine T (ST)
- DOI
- 10.2991/aeece-15.2015.52How to use a DOI?
- Keywords
- CdS; heteropolyacid; composite material; Safranine T; photocatalysis
- Abstract
A series of phosphotungstic acid and phosphomolybdic acid loaded CdS composites (HPW/CdS and HPMo/CdS) were prepared by impregnation method, and then characterized by FT-IR, XRD and TEM. The influences of different loading amounts on degradation rate of Safranine T under ultraviolet (UV) light irradiation were discussed. And, the changes of absorption peak and absorption intensity of Safranine T (ST) solution during the degradation process was monitored on UV-Vis spectrometer. The results show that synergistic effects exist in HPA/CdS and lead to improved photocatalytic degradation effects in comparison with corresponding CdS or heteropolyacid. HPMo/CdS with mass ratio of HPMo of 30 wt% exhibiting the best photocatalytic activity for degradation of ST under acid condition, with the degradation rate of 84.3% under UV light irradiation for 120 min, and UV-Vis spectrum show that new substance is formed during the degradation process.
- Copyright
- © 2015, the Authors. Published by Atlantis Press.
- Open Access
- This is an open access article distributed under the CC BY-NC license (http://creativecommons.org/licenses/by-nc/4.0/).
Cite this article
TY - CONF AU - Shuang Song AU - Long Fan AU - Shuyuan Xie AU - Jinghai Liu AU - Limei Duan PY - 2015/09 DA - 2015/09 TI - Photocatalytic Heteropolyacid/CdS (HPA/CdS) Composite for Degradation of Safranine T (ST) BT - Proceedings of the International Conference on Advances in Energy, Environment and Chemical Engineering PB - Atlantis Press SP - 257 EP - 262 SN - 2352-5401 UR - https://doi.org/10.2991/aeece-15.2015.52 DO - 10.2991/aeece-15.2015.52 ID - Song2015/09 ER -